Hi folks,

This is a general question regarding the strength and rigidity of a wet layup. Would there be any mechanical difference in the finished item using fewer laminations of a heavier weight glass than more of a lighter weight, i.e. 3 @ 200g as opposed to 2 @ 300g.




Cheers, Marty
Reply
Martin Fraser
Martin Fraser
Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)
Group: Forum Members
Posts: 11, Visits: 148
Hi Warren,

Thanks for that.  The tail pylon section is about 500mm long and the OAL of the model is 1840mm - see attached. 

I've done another pull of it yesterday but laid a 50g twill down first. It's so thin that I could check for air pockets even though the resin was tinted. I then let this tack off for an hour or so and then followed up with one 100g and three 200g layers alternating their weave direction. I had a gentle heat on (70*) it for 8 hours The finish is perfect but it still feels a bit flexi? Might do one in clear resin and compare.

Cheers, Marty
Attachments
Moulded.jpg (707 views, 145.00 KB)
Plug glossed.jpg (740 views, 88.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search