Hi,

I am a begginer in carbon fiber and I am currently facing a problem. I have a mould that is similar to a U shape so when I apply the fist coat of epoxy resin it falls from the almost vertical sides and creates a pool in the middle, is there any tip to make the epoxy resin more viscous so it will not fall down?

Also I would like to include an image in the front cover of the carbon fiber as seen on the picture below. I have tried using lacquer after the carbon fiber part is done and did not work. I tried placing the image as a first layer in the mould before any carbon fiber, but it did not work either since the first epoxy layer did not adhere to the image. Any ideas how can I make this? I was thinking on pasting the image once the carbon fiber part is made and then apply a thick coat of epoxy resin on top of it, but I fear it will drip down and would not leave a uniform layer.

http://www.talkcomposites.com/Uploads/Images/ce4c7c0f-554a-4bdc-9412-44c3.JPG


Thank you in advance,
Reply
joacomogollon
joacomogollon
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 14
Thank you guys for the help.

Hanaldo: What type of clear coat will you recommend? 

Dravis: For the gel coat would you reccomend the GC50Epoxy compatible Gelcoat? Thank you for the warm water bag it's a good tip.

brainfart: I do not know exactly the material of the paper, but do you think it may help for the adhesion if I give the paper a varnish coat before getting in contact with the epoxy resin?