Hi

Need some help on this one as keep getting circle marks on finished items when using a sander machine. Any other options as i find its tiring to use manual sanding on large items ie. motor fairings
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi,

If this relates to a specific Easy Composites product (Mirka Polarshine polishing compound for instance) then please state which product (C20, T10, F05 etc.) so that I can give you the right advice. If it's just a general question about flatting and polishing then just let me know and I can move this thread into the main forum where I'm sure your fellow members will be happy to help.

Kind regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
fx3861
fx3861
Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)
Group: Forum Members
Posts: 9, Visits: 49
sorry its a general question as i tried using a sand machine to flatten and smoothen the carbon parts