hi guys,
i'd like to ask you if somebody has some experience with Diolen and with his look after coating.
After applying of top coat I am observing an unequal pattern or texture on surface from Diolen. Diolen fabrics itself looks good but after applying of top coat some strings of fibre
are darker than others. The more top coats the worst effect.
steps in skinning:
- black base coat then diolen
- 1st layer of top coat >>> images 1st layer.jpg
- 2nd layer of top coat + Lacquer >>> images 2nd layer

on pictures are different parts of skinned parts.
when I used only 1st layer of top coat the lines are visible but not so much.
after applying of 2nd layer the "lines" are visible too much.

Could it be a faulty Diolen product?
I tried to apply top coat with brush and also with plastic card but still with the same effect.

any help or advice is more than appreciated.
thank you very much
ondrej
Attachments
1st layer.jpg (1.6K views, 964.00 KB)
1st layer_2.jpg (1.5K views, 67.00 KB)
2nd layer.JPG (1.8K views, 44.00 KB)
2nd layer_2.JPG (1.8K views, 42.00 KB)
Edited 14 Years Ago by odo
Reply
odo
odo
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Awaiting Activation
Posts: 5, Visits: 66
Hello Paul,

thanks a lot for help! Now we have a car in carservice, when it comes back i'll make order from easycomposites.
thank you again
have a great day!
ondrej
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search