Box Section Average weights
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
rgallagher27
rgallagher27
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 5
Could you give me an idea of the average weight of 2m * 20mm Carbon Fibre box section
Cheers,
Ross
Reply
Like
8
Reply
Dravis
Dravis
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Box Section Average weights
rgallagher27
-
12 Years Ago
You can calculate it :-) The density is between 1,3 and 1,5 grams per cubic centimetre .. 200 cm x...
Dravis
-
12 Years Ago
Just measured a piece and it is 326g for a 2m length.
Warren (Staff)
-
12 Years Ago
:D :cool:
Dravis
-
12 Years Ago
Thought you'd be pleased your calculation was spot on LOL.
Warren (Staff)
-
12 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search