Well, here it is Smile The customer just collected this little beauty

Base


Deck


With my new System bindings attached Smile (just for effect!)

kidpaint
kidpaint
Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)
Group: Forum Members
Posts: 99, Visits: 676
looks great. Is building these similar to the process of building a snowboard?
Blackrat
Blackrat
Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)
Group: Forum Members
Posts: 20, Visits: 85
whats the layup on the board ?
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Ah, that would be telling!!!! lets just say it varies a lot and it's highly engineered Wink



Kidpaint, pretty similar but I use a forming mould with vacuum bagging & heat rather than a heated press