I want to make a protection for my musical instrument


Author
Message
tdanr
tdanr
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 2, Visits: 26
Hi Smile

I have a musical instrument that has a protective metal. The protection is very good, but it is very heavy, i need a lighter protection.

You can see in photos:

http://www.talkcomposites.com/Uploads/Images/1006ebd5-bf50-4864-a7a0-7b9d.JPG http://www.talkcomposites.com/Uploads/Images/af80c5c3-a07a-45fd-bdbd-7909.JPG

I think to make a protection using this method:
http://youtu.be/v4SPPtYaN8w

I'm thinking using the metallic protection as a template/guide/mould, is possible?

What is the fabric and the resin advised?

I saw some fabric and I think these are the nominees:

Carbon Fibre 2/2 Twill 3k 199g 1m Wide

Carbon Fibre 2/2 Twill 12k 450g 1m Wide

Carbon Fibre 2/2 Twill 12k 650g 1m Wide

Carbon Black Twaron 200g 2/2 Twill 1m Wide

Carbon Aramid 2/2 Twill 3k 210g 1.2m Wide

Aramid Cloth Fabric 2/2 Twill Weave 300g 1m Wide



I do not know what the best resin for this method, maybe EL2 Epoxy Laminating Resin.

Someone can give me some help?



Thank you

Regards


Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Pretty much all covered!

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant