Hi,



1. 

I need to make an 110 x 40 x 0,4 cm water clear resin cast. Would you recommend polyester resin for this ? The mould I will use is made of rtv silicone.


2. 

I will cast in an open mould. 

Any suggestions on how I can keep the surface of my cast tack free ? 

I read that cellophane film can be used to cover the surface of the cast and protect it from air. If this is correct: Do I need to place the cellophane film DIRECTLY on the surface after I have poured the resin ? Or will it do if I place the cellophane 1 cm over the surface ? (My mould is in a wooden frame, and it would be a lot easier to place (tape) the cellophane ON the frame, rather than IN the frame.) 

If I need to place the cellophane film directly on the surface: When do I do that? Immediately or when the resin has started to cure?

I also read about MW wax. If that would be a better idea for protecting the surface: how do I apply the wax ? Do I mix it with the resin, or do i pour it over the resin as a final layer ?

I need a clear and transparent cast without any cloudiness or discolouration.


Thank you




Edited 11 Years Ago by palace
Reply
palace
palace
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 6, Visits: 41

Well, one side of my cast will be against the silicone mould, which has a lot of complex details. The other side, the one that is in the open, will be the back of the cast.


brainfart (17/08/2014)

>
I need to make an 110 x 40 x 0,4 cm water clear resin cast.

Just buy a sheet of clear acrylic/plexiglas at the next hardware store. Much cheaper, easier, faster.

Edited 11 Years Ago by palace
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search