Is it possible to machine carbon laminates in a similar fashion to metals, ie turn on a lathe?  I am considering some mouldings that need some serious accuracy with wierd shapes and I was thinking this might be another option.
Reply
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
No problems machining it but you will find lots of machine shops are against it

Some on the grounds of dust extraction others don't like carbon dust on the beds of the machines and in the workings