Hi all , new to all this but since i've got a plastic car that needs repairing thought i would join up to tap into the knowledge on here .

 My question is what resin to use to join the front edge of the crash box , it looks like carbon but googling shows its GRP, i have the part cut out of another one just wondering what resin would be best to join them and then would a carbon tape help to strengthen the join .

 if it was huge damage i would replace the whole thing but the tech manual says repairs to the lip is ok

Cheers
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Hmmm, you're a fair way from me I'm afraid.  Best of luck with the fix though. 