Why is 12k carbon fiber tow more expensive than 12k Woven Carbon Cloth on a per kilo basis?


Why is 12k carbon fiber tow more expensive than 12k Woven Carbon Cloth on a per kilo basis?
Author
Message
drivingsouth
drivingsouth
Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)
Group: Forum Members
Posts: 1, Visits: 8
I'm comparing
- 12k carbon fiber 4,5kg tow
- Carbon Fibre 2/2 Twill 12k 650g

On a per kilo basis, using the best price on bulk, tow is 37.7 GBP Kg per kilo and cloth 32 GBP.

This doesn't seem to make make sense since cloth is tow cost + cloth making costs (machinery,etc..). Am i seeing anything wrong?
Reply
brainfart
brainfart
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
It's only illegal if you want to export to IRANSYRIASUDANNORTHKOREA, because that would make you an EVIL TERRORIST SUPPORTER (TM)