Hi,

I was wondering if this profile is the only one that you produce, as I have a pressure pot setup with a very specific internal geometry.
If not, are you able to forward me on to the company that produce these liners for you?

Kind Regards,

James Stefanou
+61 407 856 684
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As long as the cup fits you will be fine.

Plan your resin feed and distribution to help avoid wastage.  Also leave a gap between the part and the vacuum feed mesh.  It helps slow down resin flow to the catchpot.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search