To be honest, for a new product i would be returning it.
simple cracks can be cosmetically filled with resin either by sanding back or flexing ans syringing fresh resin in, then sanding to match and polishing back up.
However you have lots and lots of cracks which is going to be many hours work.
Also any that have gone right through to the reverse as well, will have compromised the strength significantly meaning you would need to add additional reinforcement to replace the lost strength where the carbon has itself broken.