Hey guys,
  Can anyone tell me how I would go about prepping this plastic fork guard from my motorcycle without the polyester tooling gel coat ruining the piece?  Painting it is not an option.

  Would I just layer the pva thick on the part since I'm not sure if mold release wax will work?

Thanks a bunch


Edited 11 Years Ago by whitecel
Reply
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
I rarely use PVA and just use Easy lease on the part and if used correctly you genuine part will be left in as new condition.
Regards Chris
Carbon fibre works LTD

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
whitecel - 11 Years Ago
Hanaldo - 11 Years Ago
whitecel - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
whitecel - 11 Years Ago
carbonfibreworks - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
Hanaldo - 11 Years Ago
whitecel - 11 Years Ago
FLD - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
whitecel - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search