	Group: Forum Members 	        
    Posts: 6, 
    Visits: 20 
    
 
          
		     | 
				                       
                 
                
                    
			            I am hoping to use carbon fibre composite tube for the pendulum of a precision regulator clock.  I believe that the coefficient of thermal expansion of pulltruded carbon fibre composite is somewhere between 0.1 and 0.3 ppm /°C but wonder if you can give a more exact figure  for your tubes so that I can design a compensator.
  Thanks in advance.
  Edit:  The coefficient is I believe negative.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |