Moulding weight opinions saught


Author
Message
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I'm just looking into making a few parts (in my usual sloooow pace) and I'm considering core materials.  I appreciate the convenience of soric however I'm looking for your opinions on ultimate weight minimisation.  I cant really use honeycombs as I have a single mould so please restrict it to common cores.  I'm looking for a comparison between thinks like soric, balsa, foam etc as to what is ultimately the lightest moulding.  I appreciate the extra labour with foam of infuse/bond/infuse but its just for myself.  My suspiscion is it will be foam, soric, balsa in order but I'm happy to be corrected.

Thanks y'all
Reply
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
FLD (13/06/2014)
I'm just looking into making a few parts (in my usual sloooow pace) and I'm considering core materials.


Without knowing more details we cannot really comment on what's the most suitable.

I appreciate the convenience of soric however I'm looking for your opinions on ultimate weight minimisation.


Aramid honeycomb.

I cant really use honeycombs as I have a single mould so please restrict it to common cores.


Sure you can use honeycombs.

I'm looking for a comparison between thinks like soric, balsa, foam etc as to what is ultimately the lightest moulding.


From light to heavy: honeycomb, certain foams, balsa, soric. Depends on the required thickness.