Hi all, after some help please…

I am making a "mould" but without an original part, its a simple item so I am making from foam core and was going to "paint it" using Uni Mould obviously using the catalyst and using the MW agent stuff, so I am mixing it as you would for doing a mould repair so it dries out.

My problem is I know if I paint brush this on to the flat surface and then look to flat it off afterwards, most of my time will be spent just rubbing out the brush stroke marks, I believe the Uni Mould is to thick to spray on so how can you apply this giving the flattest finish??

I am thinking of using a paint brush to apply it and then using a roller to get a better flat finish prior to rubbing it down. Has anyone done this before and can pass on their advice please?

Cheers,
Lee.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Hmmm, this is going to be a hell of a lot of work no matter what way you do it I'm afraid. There just isn't a way to apply it smoothly enough that you can get away without rubbing it down, and gelcoat is very hard so it isn't easy to flat. Perhaps with a DA sander you may save some hours, but even then... May I ask how you intend to apply your reinforcement? 

Why do you not use your foam core as the male version and make a female mould? 
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Does it have to be gel coat? If you're trying to make a smooth hard surface for the part, you could mix up poly resin and talc which is easy to sand and sets hard
Toffee
Toffee
Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)
Group: Forum Members
Posts: 36, Visits: 118
Hi guys, its just a 200mm wide channel I am making, rather than using EC Primer I thought I would have a go at using the mould making materials as this is what it is designed for, maybe not the application, but as a surface for a mould. I know I will still have to do some rubbing down, but as you've stated its tough stuff and takes some rubbing. I do have a DA sander which helps, but its the application using a brush that makes it so much work, there must be a better way of applying this so the surface is flatter??
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You could try applying it by brush, then using a spreader to flatten it out some. But even that is going to be frustrating.

What are you trying to achieve by skipping the prep of the plug? I dare-say you will spend more time trying to flat the unimould than you would the pattern primer, and you still won't get as good a result. 
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
My first question on using the unimould gelcoat would be can it fully cure when exposed to an "air" environment? Most gels won't (well poly gel won't) I've not tried a vinylester  gel before so don't know the ins and outs of it.

If it's "just a simple channel" then why not just make a male (or female) box out of MDF or HDPE?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
He did say he would be using the wax additive so it cures hard. 

OP, it might help if you detail what you are trying to achieve, but I really do think using the Unimould is the hardest way to go about it. 
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Ah, didn't spot that....