MEKP shelf life and disposal?


Author
Message
Leew
Leew
Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)
Group: Forum Members
Posts: 33, Visits: 187
Hi, I have some MEKP catalyst which is 3-4 years old.  Is it safe to use this in a new project or could it have "gone off" and thus ruin my project.  MEKP is cheap enough so if there is any risk it won't work and I need to buy some more then that's ok.  If I do need to dispose of this MEKP, what is the recommended way of doing it?  I know MEKP is really nasty stuff (I belive it is about the nastyest chemical used in composites), so want to make sure I dispose of it properly and safely.

Many thanks, lee.
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
The answer is easy, make a small batch and see if it works or not Smile 
About throwing it away I would have no clue, would be interesting to hear whats the best way

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com