Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Carbon Fiber Race Seat
Carbon Fiber Race Seat
Post Reply
Like
2
Carbon Fiber Race Seat
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
wochi
wochi
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 31,
Visits: 188
Hi all,
i´m trying to do a race seat for my car buy i have no idea of how many layers i should apply to make a good compromise between cost/weight/rigidity.
I was thinking in carbon/glass/soric/glass/carbon but no idea of how many layers and grams of each one.
Anyone can help?
Thanks in advance!
David
Reply
Like
2
Reply
wochi
wochi
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 31,
Visits: 188
you can insert some metal plates between the layers when infusin and then drill
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon Fiber Race Seat
wochi
-
11 Years Ago
I generally encourage the creative process...except when your safety might be in jeopardy. Think...
BlackNDecker
-
11 Years Ago
I can´t see why. I see many people using Ebay seats that everytime you seat it seems that is cracks...
wochi
-
11 Years Ago
[quote][b]wochi (30/05/2014)[/b][hr]I can´t see why. I see many people using Ebay seats that...
BlackNDecker
-
11 Years Ago
Because without crash testing, you don't know if you've got something something decent. A lot of...
Hanaldo
-
11 Years Ago
http://www.youtube.com/watch?v=aF3ll_h9EAw The video shows infusion of a seat, and what material...
brainfart
-
11 Years Ago
For safety critical componants generally if you cant have it tested or lack the facilities/know how...
Warren (Staff)
-
11 Years Ago
I can´t see why all this trouble with the seat. I´m aware that is a safety part but a door, an...
wochi
-
11 Years Ago
Yes but a bonnet or door isn't going to be the difference between you walking away from an accident...
Hanaldo
-
11 Years Ago
If you have an accident and the door breaks you will probably have razor blades in your direction so...
wochi
-
11 Years Ago
There is a good example of a carbon seat in "Composite Materials Fabrication Handbook #2" by John...
ChrisR
-
11 Years Ago
I have that book. And it´s a good starter but the seat is very small so I´m affraid that the layup...
wochi
-
11 Years Ago
I think you are underestimating the strength and stiffness you can get from CF, the layup suggested...
ChrisR
-
11 Years Ago
[quote][b]ChrisR (30/05/2014)[/b][hr]I think you are underestimating the strength and stiffness you...
wochi
-
11 Years Ago
While I stand by my previous posts, this is in addition... [quote][b]wochi (30/05/2014)[/b][hr]If...
ChrisR
-
11 Years Ago
[quote][b]ChrisR (30/05/2014)[/b][hr]While I stand by my previous posts, this is in addition......
wochi
-
11 Years Ago
As far as I read above they are not commanding you not to do it, it's more like it's kind of a risky...
matthieutje65
-
11 Years Ago
How are you going to incorporate bracket holes for mounting? You won't be able to drill directly...
BlackNDecker
-
11 Years Ago
you can insert some metal plates between the layers when infusin and then drill
wochi
-
11 Years Ago
Hello Wochi, What I do not understand with you is you come on to the Forum for...
The Fibreglass King
-
11 Years Ago
[quote][b]The Fibreglass King (30/05/2014)[/b][hr] Hello Wochi, What I do not...
wochi
-
11 Years Ago
I'm not totally totally sure if it matters, but if I were making it I would be putting the aramid...
Hanaldo
-
11 Years Ago
Couple of things to think about are try a peel test between the Kevlar and the soric and the carbon...
f1rob
-
11 Years Ago
This is why I love forums. Always something to learn! Was not aware of the bonding issues between...
Hanaldo
-
11 Years Ago
doesntmatter what it is 90g satin/200g the bond on a Kevlar is always worse than anything else...
f1rob
-
11 Years Ago
Now that´s a good discussion! Thanks a lot for all the help! So with the materials I have with me...
wochi
-
11 Years Ago
I would be interested to hear more discussion on molding in the bracket hardware. There has been a...
BlackNDecker
-
11 Years Ago
I've done some research & testing on this and the results are quite interesting. When I get some...
ChrisR
-
11 Years Ago
[quote][b]ChrisR (16/06/2014)[/b][hr]I've done some research & testing on this and the results are...
BlackNDecker
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search