			            For safety critical componants generally if you cant have it tested or lack the facilities/know how to do a proper structural design and strength calculations, then Generally we recommend you get someone to make it for you.
 However, if you copy something similar that you know is safe (in terms of general layup etc) and over engineer it a bit then you should be ok - but it is still a risk you have to understand.
 