Hi guys
For those of you how are experienced this is probably a stupid question but I'm gonna ask anyway as I suspect it is something many struggle with.
What is your technique for getting a good finish on your plug?
I have a GF part which I want to take mould from, this is it although I have worked at it since these photos were taken.




I wanted to make a copy of my cracked instrument binnacle but it was very textured so I smoothed it as best I could and made a mould from it (actually I made four as this was my
first ever go at doing this and I didn't really know what I was doing) I then made a GF part from the least worst of the moulds and set about smoothing it. I started with 120 grit, then went on to 400, 800 and 1200.
My plan is to take this part which apart from the scratches I am happy with and make a new mould in two or three parts (advise on this very welcome) so that I can make CF copies which I hope to sell.
I thought it was going well until I rubbed it with cutting compound to a nice shiny finish but when I looked closely it was covered in lots of scratches, probably from the last two grits.

So, do you wet sand or dry sand?
How can you tell when you have sanded away the marks left by the previous grit? I dried it and thought they were gone but apparently not.
Do you use a DA sander, a block or just hold the paper?
How long do you normally spend smoothing a part like this, I spent a whole evening at it and will probably need to spend another one to get rid of the fine scratches.
How smooth a finish is realistic on Gel coat?

Thanks in advance
Ali
Edited 11 Years Ago by Alibro
Reply
Alibro
Alibro
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 44, Visits: 384
Thanks for the replies guys, I had four goes at making a one piece mould but it got locked each time. The last time it was so bad I cracked the plug getting it out but I think that was because I made the mould better (ironically).
The flange with the holes and bumps is structural so I think I will do as Hanaldo suggests and put the barrier to the edge of the main part.
I will report back when I get it done.
I would like to try the Pattern Hi gloss but will need to wait until I am ready to put in a big order as the postage price to Northern Ireland is to high for a single part.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
Hanaldo - 11 Years Ago
Alibro - 11 Years Ago
The Fibreglass King - 11 Years Ago
Hanaldo - 11 Years Ago
Warren (Staff) - 11 Years Ago
Alibro - 11 Years Ago
FLD - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
tack talk - 11 Years Ago
Alibro - 11 Years Ago
Hanaldo - 11 Years Ago
Warren (Staff) - 11 Years Ago
Alibro - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
brainfart - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search