Flox mixture ratio


Author
Message
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi Guys
I was watching a youtube video of a German company building gliders (sailplanes)
They were mixing a adhesive that they were gluing the wings together with.
I am assuming that it was composed of Sad my guess)  Epoxy/ flox/ cabasol/ milled glass fibers.
If anyone knows for sure I would really appreciate the formula.
The ingredients and ratio please.
Thanks
Fred
Reply
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
The standard resin nearly all of the German glider and small aircraft manufacturers use is the blue one, Epikote MGS L285.

www.pylon-line.co.uk/td_en_LR285_eng_180310.pdf

The name might have changed a little (or maybe not since it's such an established brand name), the original German manufacturer (MGS) was bought by Hexion (that's where the Epikote comes from), which then became Momentive and in 5 years they will probably change their name once more...

Very nice material, unfortunately only fast hardener is still available to the public thanks to the chemophobia of our lovely European Union. If you have a business you can of course still buy them all with no hassle, just don't get caught reselling it to the general public in larger amounts. I really like this resin a lot, it's a bit more expensive than all the standard laminating resins but not prohibitively more especially when you buy larger amounts from distributors and volume discounts become available. This is only valid for Europe of course, I know that it is quite pricey and in occasionally not available in the US since it has to be imported from Germany. Courious to say the least, since Hexion/Momentive is based in the US.