Hi guys,

I made a stupid mistake today and I thought you would like to see it.
 
I was mixing Uni-Mould tooling Gel Coat and thinking to myself "50 grammes seems like a lot of M.E.K.P. Oh ****! It should have been 5 grammes"
I put the mixture outside by a bucket of water grabbed an Infra red thermometer and my camera. After a few minutes it got up to 60 deg C. I dropped it in the bucket and filmed it.

Brian.

http://youtu.be/cG6m8Zt9KM0
Edited 11 Years Ago by Brian_s