Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
New technique a bit like skinning?
New technique a bit like skinning?
Post Reply
Like
3
New technique a bit like skinning?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
racitup
racitup
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 13
Hi everyone,
I'm new to this, I just started watching some videos on Monday so I've no idea if this is a new idea or not, but I'm interested in copying some car parts without making moulds.
The idea goes something like this:
Cover the part in release agent then single sided prepreg, epoxy side out and secure edges with tape or temporary glue
Cover the prepreg tightly (no air bubbles) with thin clear flexible heat resistant gloss sheet gloss side in; e.g. silicone or latex
Seal the sheet behind, either to itself or a backing with vacuum connection
Cure it in an oven
Remove the laminate from the original
Add extra layers inside the first and cure using whatever technique you fancy
Gotchas:
The part has to be good for 100ish degrees
Would the epoxy stick to the silicone and does anyone know if latex would work?
BTW really excellent Easy Composites videos, infusion is so impressive.
Rich
Reply
Like
3
Reply
racitup
racitup
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 13
Hi guys,
Thanks for the responses.
Fasta: Great points about expansion at 100degC and suitability for releasing
Hanaldo: I was only thinking of making one copy of several parts for myself. Making moulds for them all would take a lot of time and money and some are very complex
Ajb: thanks for sharing. A couple of panels are fairly flat so this could work. Sounds like infusion would be the way to go to eliminate temperature related problems...
Since I've had such a good response, could anyone advise on what they think would be the best method of copying the original plastic grilles from a Lotus Elise S2 in carbon fibre?
Alternatively is there anyone that would do this for me maybe, preferably based near Warwickshire?
Cheers,
Rich
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
New technique a bit like skinning?
racitup
-
11 Years Ago
So basically you are wanting to mould anew thin partfrom the outside of a part you already have. I...
Fasta
-
11 Years Ago
Is there a reason you want to avoid making a mould?
Hanaldo
-
11 Years Ago
I think it will work, but only for relatively simple flat shapes. The difficulty will be preventing...
ajb100
-
11 Years Ago
Hi guys, Thanks for the responses. Fasta: Great points about expansion at 100degC and suitability...
racitup
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search