Ive given some resin infused parts to a paintshop for clearcoating

Overall the surface is pretty good, some areas of porosity,pinholes but its minor.

 

My guy prepped with 1500 grit, scotchbrite and degreased.

He put on several coats and had issues with pitting, unevenfinish.

 

Wondered if anyone had any input or ideas on process andpreparation.

Whenever i have done any small parts myself i went for600/800 grit prep, couple coats of lacquer, then 1000/1200 grit and finallacquer coats.

Im wondering whether the 1500 is not enough grit, and the lacquer is seperating/repelling

 

Please see pics attached 


Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I've been struggeling a lot with 2K spraypaint as well...
still working on it BigGrin FLD can you tell me with what you dilute the 2K clear with?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com