Can you please provide some guidance numbers on the corner radius of box sections.

If there are CAD diagrams that would be great.

Specifically looking for corner (inner and outer) radius of 20mm box section.

I need to prepare an accurately fitting mating component.

thanks
Krishna
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
HI,

The 20mm box section does not have any CAD drawings available to us.  It is not massively precise.  The internal radii seems to vary between 3.6 and 3.8mm.  The outer radii varies between 4.8 and 5.2mm.  That has been measured by hand.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ksanjeev
ksanjeev
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 2, Visits: 9
Thanks Warren. This data is sufficient for my needs. 
Krishna
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search