Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Resins, Gelcoats and Pigments
»
Ethanol Resistant Resins
Ethanol Resistant Resins
Post Reply
Like
9
Ethanol Resistant Resins
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TrialsIron
TrialsIron
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 8
Hi there
I'm relatively new to using composites and not familiar with the different types of resins available. I am looking to make fiber glass petrol tanks for competition motorcycles. There are a lot of people already using these on the Pre65 Trials circuit but in the last few years a lot of them have started to delaminate and bubble. Additionally the resin has been clogging up the carburettors. This is attributed to the Ethanol in modern fuels.
Is there a resin available that is resistant to ethanol even at the quantities used in E85 which has yet to reach our shores.
Many thanks
Steve
Reply
Like
9
Reply
kidpaint
kidpaint
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 676
idk if this is what you are looking for but a local supplier by me just posted this on their site. Might be worth a call to see if it fits your application. Sorry EC, I know this is another vendor, Im not promoting just trying to help.
http://expresscomposites.com/NEW.html
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Ethanol Resistant Resins
TrialsIron
-
12 Years Ago
Hi there I to have just finished making carbon tank with Kevlar before I bond the parts together I...
Shaneer22
-
12 Years Ago
Many thanks for the advice. I was really hoping to laminate with it but I might have to settle for a...
TrialsIron
-
12 Years Ago
here is what i found ethanol friendly tank lining materials
brasco
-
12 Years Ago
more info on this isssue but in boats. it goes into technical details of what is chemically...
brasco
-
12 Years Ago
We don't stock any resins designed for petrol tank and ethanol resistance. You would likely need to...
Warren (Staff)
-
12 Years Ago
Hi Warren - thanks for your reply. About a year ago I read about a Phenolic resin that was allegedly...
TrialsIron
-
12 Years Ago
Im no expert by any means but it sounds to me like the expoxy must be sealed away from the fuel....
pk_090
-
12 Years Ago
There is a big difference between occasionally pouring fuel over paint and soaking in it 24/7.
Warren (Staff)
-
12 Years Ago
I suppose yes, good point Warren.
pk_090
-
12 Years Ago
We would unlikely have any more resources than yourself and the power of the internet. We have...
Warren (Staff)
-
12 Years Ago
How did your brake fluid tank hold up warren? Brake fluid is nasty to normal paintwork have you had...
pk_090
-
12 Years Ago
It's not finished yet! LOL. Too many projects on the go and working a lot more now. However the...
Warren (Staff)
-
12 Years Ago
Here is to bringing life to an old post. In the aviation industry tanks they tend to use...
20_rc51_00
-
11 Years Ago
I am using an ethanol resistant resin to both seal the inside of the pre-preg tank and initially I...
morepower
-
11 Years Ago
Personally I would look into making a custom bladder for the inside of the mold, like pretty much...
combustioncraig
-
11 Years Ago
Made a few of them and if you have the correct resin there is no problem.. The resin I use has been...
morepower
-
11 Years Ago
idk if this is what you are looking for but a local supplier by me just posted this on their site....
kidpaint
-
11 Years Ago
I'm not sure but I seem to remember that POR-15, a common metal gas tank sealer works on epoxies...
brainfart
-
11 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search