I have completed my mould and would like to do the resininfusion.

Could someone please advise me on the correct location forthe resin inlet and vacuum line?

ShouldI maybe place the resin line in the middle from right to left and the vacuumline around the edge?

Anyideas?


Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Agree with above. I would also run the spiral round the corners and up the short sides and use two resin feeds spaced along the long side.

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search