Group: Forum Members
Posts: 156,
Visits: 14K
|
Shape like that it doesn't really matter shortest or longest,as long as your resin has a longer open time meaning harderner. Again use peel ply as a resin break that way hardly any resin enters vaccum side,as long as your not in a rush use a harderner with a working time of 2 to 3 hours demoulding is around 3 days depending on working temperature good luck.
|