I have completed my mould and would like to do the resininfusion.

Could someone please advise me on the correct location forthe resin inlet and vacuum line?

ShouldI maybe place the resin line in the middle from right to left and the vacuumline around the edge?

Anyideas?


Reply
Djekouk
Djekouk
Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)
Group: Forum Members
Posts: 30, Visits: 987
Johan (27/02/2014)

I have completed my mould and would like to do the resininfusion.

Could someone please advise me on the correct location forthe resin inlet and vacuum line?

ShouldI maybe place the resin line in the middle from right to left and the vacuumline around the edge?

Anyideas?



whats the dimensions of the mold?