Can you let me know how rigid this product is?  I want to make simple flat bench 1100mm x 400mm x 100mm for a boat.  It should be able to bear 90Kg.
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
This is rigid PU foam block.  rigidity is subjective and all depends on the laminate, how it is supported etc etc.  This low density block is primarily designed for pattern making rather than as a core material. The High Density PU foam block is certified as a core material for marine use.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search