Confusion in deciding on epoxy resin


Author
Message
Krokc
Krokc
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 4, Visits: 13
Hullo everyone my name is Kumar Ranjan. I am working with a formula SAE team.
We are planning on making a carbon fiber body for our next car. In this regard I found out some suitable epoxy resin grades namely Bisphenol F and A. But when I visited suppliers website the names of epoxy were different. As on "easycomposites" epoxy resins are named as EL2 IN2.

How do I differentiate what epoxy I actually need?
Reply
Krokc
Krokc
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 4, Visits: 13
Thanx joe.

I considered your advice and posted it in the correct place.

Well I am planning to go for hand layup.