Confusion in deciding on epoxy resin


Author
Message
Krokc
Krokc
Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)
Group: Forum Members
Posts: 4, Visits: 13
Hullo everyone my name is Kumar Ranjan. I am working with a formula SAE team.
We are planning on making a carbon fiber body for our next car. In this regard I found out some suitable epoxy resin grades namely Bisphenol F and A. But when I visited suppliers website the names of epoxy were different. As on "easycomposites" epoxy resins are named as EL2 IN2.

How do I differentiate what epoxy I actually need?
Joe
Joe
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi, welcome to the forum.

You should create a new topic here, as it will be easier seen than in the new member section.

Let us know if you want to laminate your part by hand or if you want to use any vacuum process. It may help deciding which resin to use.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Krokc
Krokc
Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)
Group: Forum Members
Posts: 4, Visits: 13
Thanx joe.

I considered your advice and posted it in the correct place.

Well I am planning to go for hand layup.