Just make sure that you haven't got an air pocket in there before you put more oil in. I did that with my vacuum pump, it just kept showing that it was minimum oil so I kept putting more and more in. Ended up putting a litre in, then when I picked the pump up to move it I obviously shifted the bubble and all of a sudden the oil level went surging up and I had to try to drain it out again. Just try tilting the pump a bit, then if it doesn't come up add some more oil.
|