kornpetpani
kornpetpani
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 132
I have been reading some information about perforated release film having many type such as P16, P31.
So, I would like to know how to choose those types ?
Reply
Like
3
kornpetpani
kornpetpani
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 132
Anybody out there ?
Reply
Like
3
ChrisR
ChrisR
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
PERFORATION Hole Size / Pattern
P .045” diameter holes, staggered on ¼” centers.
P1 .045” diameter holes on ½” centers.
P2 Small slashes on ½” centers.
P3 .015” diameter holes on ¼” centers.
P4 .045” diameter holes on 2” centers.
P5 .045” diameter holes on 3 ½” centers.
P6 .015” diameter holes on 2” centers.
P3/7 .015” diameter holes on 3 ½” x 7” centers.
P8 .015” diameter holes on 8” centers.
P11 .015” diameter holes on 1/8” centers.
P31 .015” diameter holes on 1” centers.
P34 .045” diameter holes on 3/4” centers.
from the last page of
http://www.silmid.com/getattachment/3cea1311-e6b2-478f-9383-a621febd6149/A5000-Release-Film-Tech-Data.aspx
The hole pattern is by trial an error and how much resin you need to bleed from the stack, a lot of people I know just buy non perforated and make their own. (I haven't tried it myself yet)
Edited
12 Years Ago by
ChrisR
Reply
Like
3
20_rc51_00
20_rc51_00
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
Might sound like a dumb question but what is the difference between non perf releas film and the vacuum bagging material? How does it do anything differently?
misread... just realize it's about perf films, feel free to ignore.
Edited
12 Years Ago by
20_rc51_00
Reply
Like
2
kornpetpani
kornpetpani
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 132
Hi 20_rc_51, it isn't a dumb question. I've been in the same situation as you before.
You can notice the different between bagging film and release film easily,
Bagging film = designed to bag
Release film = designed to release
You can't not use release film in bagging purpose ....
I hope you will get better.
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Not sure about that one kornpetpani,
I think its possible to bag with a releasfilm (non-perforated ofcourse)
most vacuumbag I use are selfreleasing as well and I use the vacuumbag as a releasefilm as wel for my prepreg parts I make
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
kornpetpani
kornpetpani
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 132
Hi Mat, thanks for info. I'm one of your FB fan page and youtube.
I watched all of videos . You're awesome
Get back to bagging film, what kind of bag that be able to release itself, please give me more detail.
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Hi, Great to hear you like my videos and so on! I'll ask my local shop who the manufacturer is of that vac bag film...
Not sure if he will give it to me (for commercial reasons
) but I'm sure someone from easycomposites could help you as well,
normally all vac bagging films are selfreasing as well!
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search