sahil.tfateh
sahil.tfateh
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 24
I need to bond Carbon Fiber Tubes to aluminium inserts.
What should be the appropriate bond gap b/w CF tube's ID and Al inserts OD???????
Tags
carbon fibre
Reply
Like
5
Reply
Zorongo
Zorongo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 40,
Visits: 330
Make an small gap. BUT enough to avoid the Al to eliminate de resin when getting into the carbon tube.
I would say someting like 0,1 to 0,2 mm gap.
Thick the resin with silica so that it´ll keep in place better than clear resin.
Remind surface preparation on both Al and Carbon.
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bonding CF Tube to Aluminium
sahil.tfateh
-
11 Years Ago
Remind carbon will corrode aluminium if in direct contact. ;) You can avoid it by using a layer...
Zorongo
-
11 Years Ago
Like Zorongo said you will have galvanic corrosion if Al and carbon are in direct contact. Then you...
combustioncraig
-
11 Years Ago
If you have access to a lathe then a knurler will put a great surface on the Al insert for adhesion:...
stuart321
-
11 Years Ago
i have taken into consideration the reaction part!! what i am concerned with is the proper bond gap...
sahil.tfateh
-
11 Years Ago
Make an small gap. BUT enough to avoid the Al to eliminate de resin when getting into the carbon...
Zorongo
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search