Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
The surface reflections will probably be caused by uneven shrinkage. Happens when the exotherm gets too hot, so perhaps indicating that you were a little resin rich. How many layers did you do in one hit? Have you got areas that might be thicker than others, ie. where sections of fibreglass overlap?
|