Totally agree, I think in mould coatings are the way to go. I use Duratec Sunshield myself, and I love it. The only parts I don't use it as an in-mould on are ones that require secondary bonding, as then I am going to bond them together, clean up the split line and spray the Duratec as a top coat. The wonderful thing about Duratec is its high-build properties mean it's very easy to fill imperfections and you can make bond lines virtually invisible.
|