LaxFriedrichs
LaxFriedrichs
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 58,
Visits: 450
Hi all,
I'm making some very simple surfaces to use as plugs. The problem is that it will take considerable time to get the surface finish up to a high gloss.
Could you tell me if plastic wrapping (ie vinyl or similar) the surface would be suitable solution?
I will be using Easylease as a release agent, and my moulds will probably have a vinylester gelcoat.
Many thanks,
Adam
Reply
Like
2
Replies
LaxFriedrichs
LaxFriedrichs
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 58,
Visits: 450
Thanks Warren, I'll try just that.
Reply
Like
2
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
LaxFriedrichs (21/12/2013)
Thanks Warren, I'll try just that.
No problem. Its a method I use quite a lot for pulling moulds from existing parts if I am unsure of the material/surface type. The last thing you want is a "sticker" and a damaged/destroyed original.
I use 3M 77, just a light misting is all that's needed to hold the bagging film in place.
Let us know how you get on
Warren
Carbon
Copies Ltd
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Wrapping plastic (ie Vinyl) as plug surface.
LaxFriedrichs
-
12 Years Ago
If the surface you want to cover is fairly flat you can stick bagging film to it with contact...
wozza
-
12 Years Ago
Thanks Warren, I'll try just that.
LaxFriedrichs
-
12 Years Ago
[quote][b]LaxFriedrichs (21/12/2013)[/b][hr]Thanks Warren, I'll try just that.[/quote] No problem....
wozza
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search