injurys or health problems using epoxy


Author
Message
jontex
jontex
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Awaiting Activation
Posts: 4, Visits: 91
I found no topic regarding injurys caused by using epoxy, so i might aswell start one as i think its pretty important to share if you have any bad experiences using epoxy, how you treated it and how you might have got it.

I recently experienced some red rashes om my thighs, forearms, and little om my stomach. I think ive got it from cutting 24h old epxy with the angle grinder and some dust got inside my clothes. Ive taken som fat skin cream that helps the rashes to heal. Ive also bought the 3M Cover all suit to wear out side my other working clothes. I hope i have no further issues with the epoxy.

cheers from sweden
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
http://www.talkcomposites.com/Uploads/Images/400a8bc5-aa9f-4420-8939-ddf1.jpg

Something different, Cutting your fingers on sharp CF :p through latex glove and skin

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com