Group: Forum Members
Posts: 680,
Visits: 1.9K
|
Hi Gearhead,
Good question. To be honest I didn't realise that the High Temp Basecoat wasn't listed on Easy Composites as well. At first we didn't list any of the specialist 'skinning' resins on Easy Composites because it was thought that the skinning process was more relevent to our Carbon Mods customers but since then we've understood that lots of customers cross over and want to single source. I'll get the HT basecoat added to Easy Composites in the next day or so.
All the best, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|