Group: Forum Members
Posts: 592,
Visits: 1.9K
|
I still had a small amount of West systems 105 leftover from my very first purchase in 2005 ... I did a test with new hardener, and it worked perfectly after more than 7 years!!
My conclusion is, that the Resin will last for years, if kept cool, dry and dark. The hardeners however will not last much more than a couple of years, even when ideally stored.
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|