I still had a small amount of West systems 105 leftover from my very first purchase in 2005 ... I did a test with new hardener, and it worked perfectly after more than 7 years!!

My conclusion is, that the Resin will last for years, if kept cool, dry and dark.  The hardeners however will not last much more than a couple of years, even when ideally stored.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
We normally state that the resins will have a shelf life of 12 months. 

However in practice often they last much longer. If you have old resins, we recommend making a test mix to ensure it will still cure before you start on using it on a project.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
rupert
rupert
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 8
Hi, i have been buy your products for a few years now. I use the EL2 LAMINATING Epoxy with AT30 SLOW hardener.
I have a bottle which is around 10 months old, its unopened but i cant find a date on the bottle. Could you please tell me weather its still good to use ? / How long it should last for ?
Many thanks Rupert 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search