I was asked to make some air tubes for a guy restoring a Suzuki World Superbike. It was from the 750cc era and he has most parts but the air tubes he had were copies of the genuine parts but weighed in at over 500grams. They were also gel coated black so he wanted carbon. It had to be the same weave and look as good as the factory part. After he asked me to do them he was given one section of the set in brand new condition for him to check out. I was sent the part and to say it was perfect would be a lie. It had pin holes in there and although it was nice it was not worth the £1600 Suzuki originally charged for the full set. 

Here are a few photos of the ones I made. 
 
Pattern ones.



weight of the pattern parts sections.


Starting lay up..




Bagged using a bagging tube through the middle of the tubes and another bag run outside the moulds then the two are sealed to each other to allow the inner bag to expand out and pull the carbon into the mould and the outer bag to seal it all and allow the vacuum fitting to be used.

Parts straight out of the mould and not even tidied up yet here... Still has the flashing from the two mould halves.


The two halves put together..

This first set did have a couple of little issues but the second set did not have any issues and the finish out of the mould was better than the original £1600 set. 


yes it has a few pin holes but it is better than most out of autoclave pre-preg finishes..
Edited 12 Years Ago by morepower
Replies
Zorongo
Zorongo
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 40, Visits: 330
Congratulations to all of you. Beautiful Works !!!




Just one question: From the pictures, it seems to me that there´s no peel ply, perforated nor breather over the laminate. Is t correct ?

I know you can avoid peel ply, but I´ve always been told or read or experienced that you need a breather in order to conduct the vacuum.

Is the vac stact just the vac bag ?! Pinch




Thanks in advance !! Wink
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Zorongo (19/12/2013)
Congratulations to all of you. Beautiful Works !!!




Just one question: From the pictures, it seems to me that there´s no peel ply, perforated nor breather over the laminate. Is t correct ?

I know you can avoid peel ply, but I´ve always been told or read or experienced that you need a breather in order to conduct the vacuum.

Is the vac stact just the vac bag ?! Pinch




Thanks in advance !! Wink


Correct I have used a none perf release film and recently I have also just used the bag to pull down.. But these are quite small parts and the bag does have some creases which do allow air off the part. It is a risk and out of 12 parts I have had 1 which I had to re-make due to the creases pulling resin both off the surface and causing nasty ridges inside the part. But one part in 12 is acceptable I guess. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
morepower - 12 Years Ago
carboncactus - 12 Years Ago
             Looks great! thanks for sharing!
matthieutje65 - 12 Years Ago
morepower - 12 Years Ago
carboncactus - 12 Years Ago
morepower - 12 Years Ago
FLD - 12 Years Ago
morepower - 12 Years Ago
Warren (Staff) - 12 Years Ago
morepower - 12 Years Ago
Magneto - 7 Years Ago
Magneto - 7 Years Ago
Magneto - 7 Years Ago
Zorongo - 12 Years Ago
morepower - 11 Years Ago