So, I have a large split mould that I'm bringing together to finally infuse. I've ran a bead of silicone between the mating flanges to help defend against air ingress. A tiny bit of silicone squeezed out onto the mould surface. 

I've cleaned it back with acetone and seek the advice of the group. I know epoxy doesn't like to play well with the other children -will there be an adverse reaction when I come to infuse? This is a complex layup with a lot of layers and I don't want to cause myself issues. Any ideas?

Thanks
Mark
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Normally silicone is selfreleasing to most materials and epoxy is normally one of them... 
What I mostly do is use a piece of isolation-tape (very cheap, you can buy it in your DIY-store in many colors) on the seam.
Then do an envelope-bagging (part totally into the bag) and everything should be fine...


Watch 8min13 to make myself a bit more clear

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
I am planning a split mould too, and was thinking I will go one of two ways. Either envelope bag the whole thing like matthieu said, probably easiest and will result in least headaches....

Or I was thinking just put a length of tacky tape between the mould halves, then bolt together. I dont know why you would even use silicon. It is horrible with epoxy. If u acetone cleaned it it should be fine. 