Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Treatment of resin to use as food container
Treatment of resin to use as food container
Post Reply
Like
3
Treatment of resin to use as food container
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 380
I've basically made a few fruit bowls that I'd actually like to store fruits in them. My question is, what kind of treatment or topcoat should I put on the bowls. Obviously food and epoxy is a no no. Some kind of a non-toxic clear coat? Thanks in advance
Reply
Like
3
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 380
Anybody?
Reply
Like
3
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Remember where is food nothing from other places has to be in that place
i think your mom told this
Reply
Like
3
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 380
Sorry, but what?!
Reply
Like
3
Leew
Leew
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 33,
Visits: 187
EC fibreglass sell a resin which they say is food safe when post cured to 80c
see
http://www.ecfibreglasssupplies.co.uk/p-1504-crystic-491-pa-resin-including-catalyst.aspx
Reply
Like
3
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
TomDesign (19/10/2013)
Remember where is food nothing from other places has to be in that place
i think your mom told this
Well said.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search