Brushed on GC50


Author
Message
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Hi, I have just painted my mould in GC50. I got it as smooth as I could with an Easy Composites disposable brush. Now it has set it looks like a ploughed field. I assume that these ridges will distort the carbon fabric and show in the finished product.
Should I try rubbing them down or fill them with GC50 thinned with acetone?
Any other suggestions would be appreciated.

Brian.
Edited 12 Years Ago by Brian_s
Reply
cpkielycua
cpkielycua
Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)
Group: Forum Members
Posts: 29, Visits: 285
Can you post spray, or does it have to be in mold before layup?