Carbon Steerin wheel project.


Author
Message
CarZoneParts
CarZoneParts
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Awaiting Activation
Posts: 7, Visits: 71

Always wanted to do steering wheel with carbon fibre bits on so decide to try this and get some experience Smile

Some time ago come across Citroen C2 VTS steering wheel which thicker then other steering wheels and have nice profile but still going to be modified and re trimmed in new leather.

Been looking for some info how to do it but didn't find much.

Will learn on my won error & mistakes.

Ordered some CF skinning resin from as-essentials but this was mine  last order from them because received parcel and hardener was missing contact them same day and still waiting since Monday Sad

Few pictures showing slow progress:






More to come .................................................

Edited 12 Years Ago by CarZoneParts
Replies
CarZoneParts
CarZoneParts
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Awaiting Activation
Posts: 7, Visits: 71
I was going to let cure in room temp. but i have range cooker oven in garage that been mofified  so i can use this to cure this.

How long do I need this to be i oven and what temp.??????

Goint to laquer for final finish.


I order this skinning resin before join this forum m8 so going to use.
http://www.as-composites.co.uk/index.php?main_page=product_info&cPath=95_207&products_id=1703
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi
Curing data for resins should be available from your supplier.
Chris
www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
CarZoneParts - 12 Years Ago
TomDesign - 12 Years Ago
CarZoneParts - 12 Years Ago
fiberpro - 12 Years Ago
truyentl - 12 Years Ago
TomDesign - 12 Years Ago
CarZoneParts - 12 Years Ago
TomDesign - 12 Years Ago
CarZoneParts - 12 Years Ago
carbonfibreworks - 12 Years Ago
TomDesign - 12 Years Ago
     ...
TomDesign - 12 Years Ago
TomDesign - 12 Years Ago
TomDesign - 12 Years Ago
CarZoneParts - 11 Years Ago
TomDesign - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search