Will it make any difference if I put it in the oven and turn the fan on? Or that doesn't work with skinning. The part is really small so it can easily fit in my oven. If so, what temperature should I set the oven at. The ambient temperature around here is 30 degrees and it takes about 6hrs for the part to fully cure. If possible, I really want to go under that time hence my question about the oven
|