Hi gents,
As the title suggests, is there a way to speed up the curing when skinning parts? I hate waiting 8+ hrs for the part to be fully cured before I can start sanding. Would baking it do anything?
Regards,
Stan
By StanTheMan
-
8/23/2013 4:39:52 PM
I put it in the oven at 50 degrees and it worked like a charm. After an hour, the resin was rock solid. Thanks gents